by pfuetze » Fri Oct 19, 2012 12:28 am
i´m using 0.02" PET-G, too.
yes, only the PETG over the diecast, there´s a video, too, where you acutally see the whole process (more or less). i´m not concerned about the increase of body size.
the hardest part is to get the diecast out of vac-pull!
plus, be sure to stuff the inside of the diecast with plasticine (i´m using the one from the kids) to safe the windows, they will take the heat from the petg and deform quite fast. a lesson learned.